Silver oxide electrical contact material and preparation method thereof
2022/08/29
Material composition (mass fraction): 5%~12%SnO2, 2%~8%ZnO, 0.5%~5%CuO, 0.1%~1%NiO, 0.1%~0.5%In2O3, 0.1%~0.5%Bi2O3, oxidized The particle size of the material is 0.1 to 10 μm, and the remainder is Ag. The raw material of the invention adopts multi-phase reinforcement, and combines the advantages of each reinforcement phase, so as to achieve the purpose of good processing performance and excellent electrical performance of the material in the production process, and meet the requirements of high-power relay composite rivet contacts, which can be partially or completely Instead of AgCdO, it is used in high-power relays!